  "description": "Polyketone fibers comprising, on the basis of the entire repeating units, 95% by mole of a repeating unit of the formula (1) shown below, and showing a minimum value (Amin(F)) of a UV absorbance of 0.5 or less in a wavelength region of 210 to 240 nm. -CH2CH2-CO-",